Microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B alloys (2019)
- Authors:
- USP affiliated authors: NUNES, CARLOS ANGELO - EEL ; SANTOS, CLAUDINEI DOS - EEL ; FERREIRA, LUCAS MOREIRA - EEL ; ALVES, MANUEL FELLIPE RODRIGUES PAIS - EEL
- Unidade: EEL
- DOI: 10.1016/j.jallcom.2019.04.172
- Assunto: ZINCO
- Keywords: Ti6Si2B; Mechanical alloying; Spark plasma sintering
- Agências de fomento:
- Language: Inglês
- Abstract: This work reports on effect of zinc and milling time on microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered (66,7-x)Ti-xZn-22,2Si-11,1B alloys (at.-%, with x = 2 and 6 at.-%). Ball milling at different times (20, 60, 180 and 300 min) was performed under argon atmosphere in a planetary ball mill from these elemental powder mixtures. Cylinder bodies with 10 mm diameter were consolidated by spark plasma sintering (1100 °C, 12 min, 20 MPa) under argon atmosphere. As-milled powders and sintered Ti-Zn-Si-B samples were evaluated by X-ray diffraction, scanning electron microscopy, energy dispersive spectrometry, laser diffraction particle size analysis, and Vickers hardness tests. It was noted a similar behavior during ball milling of Ti-Zn-Si-B powder mixtures. Only the α-Ti and Si peaks were indexed in XRD patterns of Ti-Zn-Si-B powders milled for 300 min. Rietveld refining indicated that the amount of amorphous structures has increased during milling up to 300 min, which was more pronounced for the Ti-6Zn-22Si-11B powders. The particle sizes of the Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B powder mixtures increased during milling from 94 (20 min) to 156 (300 min) μm and from 101 (20 min) to 136 (300 min) μm, respectively. Coherently, the average specific surface area of powder particles was continuously reduced during milling. Despite the adopted parameters, the SPS process produced dense Ti-xZn-22Si-11B (x = 2 and 6 at.-%) alloys with 98% from their theoretical specific mass. Regardless of milling time, the Ti6Si2B formation was inhibited in microstructure of the spark plasma sintered Ti-6Zn-22Si-11B alloy previously milled for longer times. EDS analysis indicated that the Ti6Si2B phase dissolved close to 1.8 at.-% Zn.Beside the TiB and Ti5Si3, the Ti2Zn and Ti3Zn (not explored) phases were also found in microstructure of sintered Ti-Zn-Si-B alloys. The Ti-2Zn-22Si-11B alloy presented average Vickers hardness values higher than 1050 HV whereas the Ti-6Zn-22Si-11B alloy varied between 970 and 1036 HV, which could be associated with the Ti6Si2B formation.
- Imprenta:
- Source:
- Título: Journal of alloys and compounds
- ISSN: 09258388
- Volume/Número/Paginação/Ano: v.794, p.615-624, 2019
- Este periódico é de assinatura
- Este artigo NÃO é de acesso aberto
- Cor do Acesso Aberto: closed
-
ABNT
FERREIRA, Nelson Damásio et al. Microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B alloys. Journal of alloys and compounds, v. 794, p. 615-624, 2019Tradução . . Disponível em: https://doi.org/10.1016/j.jallcom.2019.04.172. Acesso em: 04 ago. 2025. -
APA
Ferreira, N. D., Leal Neto, R. M., Filgueira, M., Ferreira, L. M., Alves, M. A. N. U. E. L. F. R. P., Ramos, E. C. T., et al. (2019). Microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B alloys. Journal of alloys and compounds, 794, 615-624. doi:10.1016/j.jallcom.2019.04.172 -
NLM
Ferreira ND, Leal Neto RM, Filgueira M, Ferreira LM, Alves MANUELFRP, Ramos ECT, Nunes CA, Santos C dos, Ramos AS. Microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B alloys [Internet]. Journal of alloys and compounds. 2019 ;794 615-624.[citado 2025 ago. 04 ] Available from: https://doi.org/10.1016/j.jallcom.2019.04.172 -
Vancouver
Ferreira ND, Leal Neto RM, Filgueira M, Ferreira LM, Alves MANUELFRP, Ramos ECT, Nunes CA, Santos C dos, Ramos AS. Microstructure and Vickers hardness of mechanically alloyed and spark plasma sintered Ti-2Zn-22Si-11B and Ti-6Zn-22Si-11B alloys [Internet]. Journal of alloys and compounds. 2019 ;794 615-624.[citado 2025 ago. 04 ] Available from: https://doi.org/10.1016/j.jallcom.2019.04.172 - Study of the influence of titanium and niobium particle size on the Ti35Nb alloy production with controlled porosity
- Mechanical Alloying and Hot Pressing of Ti-Zr-Si-B Powder Mixtures
- Sintering behaviour of Co-28%Cr-6%Mo compacted blocks for dental prosthesis
- Zircônia estabilizada com ítria para aplicações odontológicas: propriedades ópticas e mecânicas
- Effect of zirconium addition on the phase transformations in as-cast and heat-treated Ti–Zr–Si–B alloys
- Creep Properties of Directionally Solidified Nb-Modified Ni-Base Superalloy, Mar-M247
- Effect of hot swaging on microstructure and properties of aged Ti-10Mo-20Nb alloy
- Corrosion resistance of aged Ti–Mo–Nb alloys for biomedical applications
- Microstructural and Mechanical Characterization of Directionally Solidified Conventional and Nb-Modified Mar-M247 Superalloy
- Microstructure and corrosion behavior in SBF medium of spark plasma sintered Ti-xZr-20Si-10B (x = 5, 7, 10, 15, 20-at.-%) alloys
Informações sobre o DOI: 10.1016/j.jallcom.2019.04.172 (Fonte: oaDOI API)
How to cite
A citação é gerada automaticamente e pode não estar totalmente de acordo com as normas