Influence of sub-surface damage evolution on low-energy-plasma-driven deuterium permeation through tungsten (2018)
- Authors:
- Autor USP: SILVA, TIAGO FIORINI DA - IF
- Unidade: IF
- DOI: 10.1088/1741-4326/aab571
- Subjects: FÍSICA DE PLASMAS; DEUTÉRIO; TUNGSTÊNIO
- Language: Inglês
- Imprenta:
- Source:
- Título: Nuclear Fusion
- ISSN: 0029-5515
- Volume/Número/Paginação/Ano: v. 58, n. 5, p. 056027/1-056027/18, 2018
- Este periódico é de acesso aberto
- Este artigo NÃO é de acesso aberto
-
ABNT
KAPSER, Stefan et al. Influence of sub-surface damage evolution on low-energy-plasma-driven deuterium permeation through tungsten. Nuclear Fusion, v. 58, n. 5, p. 056027/1-056027/18, 2018Tradução . . Disponível em: https://doi.org/10.1088/1741-4326/aab571. Acesso em: 26 jan. 2026. -
APA
Kapser, S., Balden, M., Silva, T. F. da, Stefan Elgeti, S., Manhard, A., Schmid, K., et al. (2018). Influence of sub-surface damage evolution on low-energy-plasma-driven deuterium permeation through tungsten. Nuclear Fusion, 58( 5), 056027/1-056027/18. doi:10.1088/1741-4326/aab571 -
NLM
Kapser S, Balden M, Silva TF da, Stefan Elgeti S, Manhard A, Schmid K, Schwarz-Selinger T, Toussaint U von. Influence of sub-surface damage evolution on low-energy-plasma-driven deuterium permeation through tungsten [Internet]. Nuclear Fusion. 2018 ; 58( 5): 056027/1-056027/18.[citado 2026 jan. 26 ] Available from: https://doi.org/10.1088/1741-4326/aab571 -
Vancouver
Kapser S, Balden M, Silva TF da, Stefan Elgeti S, Manhard A, Schmid K, Schwarz-Selinger T, Toussaint U von. Influence of sub-surface damage evolution on low-energy-plasma-driven deuterium permeation through tungsten [Internet]. Nuclear Fusion. 2018 ; 58( 5): 056027/1-056027/18.[citado 2026 jan. 26 ] Available from: https://doi.org/10.1088/1741-4326/aab571 - Início de operação e caracterização do sistema injetor do Mícrotron do IFUSP
- Growth Evolution of AZO thin Films Deposited by Magnetron Sputtering at Room Temperature
- Research on micro-patterned gaseous detector and applications
- Sistema de monitoramento de feixe baseado em radiação óptica de transição (ROT)
- Material erosion and deposition on the divertor of W7-X
- Evaluating crystal-orientation-dependent properties on polycrystalline tungsten: Example oxidation
- Calcination does not remove all carbon from colloidal nanocrystal assemblies
- Interdiffusion and phase formation at iron-tungsten interfaces
- Deuterium retention in tungsten based materials for fusion applications
- Self-Regulated Porosity and Reactivity in Mesoporous Heterogeneous Catalysts Using Colloidal Nanocrystals
Informações sobre o DOI: 10.1088/1741-4326/aab571 (Fonte: oaDOI API)
Download do texto completo
| Tipo | Nome | Link | |
|---|---|---|---|
| Kapser_2018_Nucl._Fusion_... | Direct link |
How to cite
A citação é gerada automaticamente e pode não estar totalmente de acordo com as normas