Source: Journal of Dentistry. Unidade: FOB
Subjects: TRATAMENTO RESTAURADOR ATRAUMÁTICO, CIMENTOS DE IONÔMEROS DE VIDRO
ABNT
ZANATA, Régia Luzia et al. Microhardness and chemical analysis of high-viscous glass-ionomer cement after 10 years of clinical service as ART restorations. Journal of Dentistry, v. 39, n. 12, p. 834-840, 2011Tradução . . Disponível em: https://doi.org/10.1016/j.jdent.2011.09.003. Acesso em: 06 nov. 2024.APA
Zanata, R. L., Magalhães, A. C., Lauris, J. R. P., Atta, M. T., Wang, L., & Navarro, M. F. de L. (2011). Microhardness and chemical analysis of high-viscous glass-ionomer cement after 10 years of clinical service as ART restorations. Journal of Dentistry, 39( 12), 834-840. doi:10.1016/j.jdent.2011.09.003NLM
Zanata RL, Magalhães AC, Lauris JRP, Atta MT, Wang L, Navarro MF de L. Microhardness and chemical analysis of high-viscous glass-ionomer cement after 10 years of clinical service as ART restorations [Internet]. Journal of Dentistry. 2011 ; 39( 12): 834-840.[citado 2024 nov. 06 ] Available from: https://doi.org/10.1016/j.jdent.2011.09.003Vancouver
Zanata RL, Magalhães AC, Lauris JRP, Atta MT, Wang L, Navarro MF de L. Microhardness and chemical analysis of high-viscous glass-ionomer cement after 10 years of clinical service as ART restorations [Internet]. Journal of Dentistry. 2011 ; 39( 12): 834-840.[citado 2024 nov. 06 ] Available from: https://doi.org/10.1016/j.jdent.2011.09.003