Fracture strength and probability of survival of narrow and extra-narrow dental implants after fatigue testing: in vitro and in silico analysis (2017)
- Authors:
- Autor USP: BONFANTE, ESTEVAM AUGUSTO - FOB
- Unidade: FOB
- DOI: 10.1016/j.jmbbm.2017.03.022
- Subjects: BIOMECÂNICA; FADIGA DOS MATERIAIS; IMPLANTES DENTÁRIOS; RESISTÊNCIA DOS MATERIAIS
- Keywords: Narrow diameter dental implants; Reliability; Weibull; Step-stress accelerated life-testing
- Language: Inglês
- Imprenta:
- Source:
- Título: Journal of the Mechanical Behavior of Biomedical Materials
- ISSN: 1751-6161
- Volume/Número/Paginação/Ano: v. 71, p. 244-249, July 2017
- Status:
- Artigo possui versão em acesso aberto em repositório (Green Open Access)
- Versão do Documento:
- Versão submetida (Pré-print)
- Acessar versão aberta:
-
ABNT
BORDIN, Dimorvan et al. Fracture strength and probability of survival of narrow and extra-narrow dental implants after fatigue testing: in vitro and in silico analysis. Journal of the Mechanical Behavior of Biomedical Materials, v. 71, p. 244-249, 2017Tradução . . Disponível em: https://doi.org/10.1016/j.jmbbm.2017.03.022. Acesso em: 13 abr. 2026. -
APA
Bordin, D., Bergamo, E. T. P., Fardin, V. P., Coelho, P. G., & Bonfante, E. A. (2017). Fracture strength and probability of survival of narrow and extra-narrow dental implants after fatigue testing: in vitro and in silico analysis. Journal of the Mechanical Behavior of Biomedical Materials, 71, 244-249. doi:10.1016/j.jmbbm.2017.03.022 -
NLM
Bordin D, Bergamo ETP, Fardin VP, Coelho PG, Bonfante EA. Fracture strength and probability of survival of narrow and extra-narrow dental implants after fatigue testing: in vitro and in silico analysis [Internet]. Journal of the Mechanical Behavior of Biomedical Materials. 2017 ; 71 244-249.[citado 2026 abr. 13 ] Available from: https://doi.org/10.1016/j.jmbbm.2017.03.022 -
Vancouver
Bordin D, Bergamo ETP, Fardin VP, Coelho PG, Bonfante EA. Fracture strength and probability of survival of narrow and extra-narrow dental implants after fatigue testing: in vitro and in silico analysis [Internet]. Journal of the Mechanical Behavior of Biomedical Materials. 2017 ; 71 244-249.[citado 2026 abr. 13 ] Available from: https://doi.org/10.1016/j.jmbbm.2017.03.022 - Microcomputed tomography evaluation of polymerization shrinkage of class I flowable resin composite restorations
- De olho nas tendências
- Surface characterization and in vivo evaluation of laser sintered and machined implants followed by resorbable-blasting media process: a study in sheep
- The effect of DLC-coating deposition method on the reliability and mechanical properties of abutment’s screws
- Clinical, histological, and nanomechanical parameters of implants placed in healthy and metabolically compromised patients
- Osseointegration: hierarchical designing encompassing the macrometer, micrometer, and nanometer length scales
- Influência do método de envelhecimento nas propriedades de uma zircônia translúcida comercial e experimental
- Clinical and histological evaluation of socket grafting using different types of bone substitute in adult patients
- Individual ceramic crowns for teeth
- Biomaterial and biomechanical considerations to prevent risks in implant therapy
Informações sobre a disponibilidade de versões do artigo em acesso aberto coletadas automaticamente via oaDOI API (Unpaywall).
Por se tratar de integração com serviço externo, podem existir diferentes versões do trabalho (como preprints ou postprints), que podem diferir da versão publicada.
How to cite
A citação é gerada automaticamente e pode não estar totalmente de acordo com as normas